ArticleLink only2013
Ni-625 superalloy foam processed by powder space-holder technique
İ Ünver, HÖ Gülsoy, Bülent Aydemir
Journal of Materials Engineering and Performance 22(12), 3735-3741 · DOI 10.1007/s11665-013-0702-0